Injection molding cost is the sum of three separate numbers: a one-time tooling charge, a per-part price that falls as volume rises, and the cost of the shots you never sell because they were scrap. SkillsProto quotes all three lines separately rather than as a single blended figure, with aluminium tooling in 7-10 days, steel in 15-25 days, MOQ 1, and DFM feedback inside 24 hours so the tooling decision is made before the steel is cut.

Why a single "molding cost" number is always misleading
Ask five suppliers what a part costs to mold and you will get five numbers that cannot be compared, because each one bundles a different mix of tooling, unit price, sample runs and freight. The tooling is one-time, the unit price is recurring, and blending them into a per-part figure produces a number that changes meaning every time the quantity changes.
The only way to compare quotes is to force them onto the same three lines: what the tool costs once, what each part costs after that, and how many parts you must buy before the two add up to less than the alternative process.
That framing also explains the most common surprise in the category. A quote that looks 30% cheaper at 500 pieces can be 20% more expensive at 5,000, because the tooling was amortised over a different quantity.
Line one: tooling, and why aluminium is not "cheap steel"
Tooling is a machined block of metal with a cavity cut into it, plus a runner system, ejector pins, cooling channels and a frame. Its cost is driven almost entirely by cavity count, part size, surface finish and steel grade — not by the part's complexity in the way most designers expect.
| Tool type | Typical cavity material | Lead time | Typical market range | Best volume band |
|---|---|---|---|---|
| Aluminium, 1 cavity | 7075 / 6061 billet | 7-10 days | Low four figures | 50-2,000 parts |
| Aluminium, 2-4 cavities | 7075 billet | 10-15 days | Mid four figures | 2,000-10,000 parts |
| Steel, 1 cavity (P20) | Pre-hardened P20 | 15-25 days | Mid to high four figures | 10,000-100,000 parts |
| Steel, multi-cavity (H13) | Hardened H13 | 25-40 days | Five figures | 100,000+ parts |
The ranges above are market ranges for the geometry described, not a SkillsProto price list: two parts of the same size can differ by a factor of three on tooling because one has a 0.5 mm rib and the other does not. The useful number is the ratio — aluminium tooling typically costs 40-60% of a comparable steel tool, and reaches first samples in about half the time.
Aluminium is not a downgrade for prototypes. It is the correct material when the tool will run a few thousand shots and the design is still moving. A 7075 aluminium cavity holds dimensions well enough for functional testing, takes a polish for cosmetic parts, and can be re-cut if a feature changes. What it will not survive is 100,000 shots of glass-filled nylon.
Line two: unit price, and the four things that set it
The per-part price is not a percentage of tooling, and it is not a fixed markup on material. It is the sum of machine time, material, scrap and finishing, divided by the parts per cycle.
1. Cycle time. Cooling dominates. A 2 mm wall cools in roughly 8-12 seconds, a 4 mm wall in 25-35 seconds, and the difference multiplied across a production run is larger than any material saving.
2. Cavity count. Four cavities cut machine time per part by roughly 75%, but they quadruple the tooling and the tonnage required. The optimum is usually one cavity under 2,000 parts.
3. Material. Commodity ABS or PP is a few euros per kilogram; glass-filled PEEK or PEI can be 30-60x more, and it wears tooling faster, which is why glass-filled parts belong in steel.
4. Runner type. A hot runner eliminates sprue waste but adds €2,000-€8,000 to the tool. It pays above roughly 10,000 parts or where the material is expensive.
Wall thickness is the single highest-leverage design decision, and it is free to change on a drawing. Reducing a 3.5 mm wall to 2.5 mm can cut cycle time by a third and remove sink marks at the same time.
Line three: the volume where molding actually wins
Injection molding has a fixed cost that CNC machining does not, so it always loses at low quantity and almost always wins at high quantity. The crossover is a calculation, not a rule of thumb, but it lands in a narrow band for most parts.
| Quantity | CNC machined | Injection molded, aluminium tool | Injection molded, steel tool |
|---|---|---|---|
| 1 | Cheapest option | Not economic | Not economic |
| 50 | Competitive | Tooling dominates | Tooling dominates |
| 200 | Expensive per part | Often at crossover | Still tooling-dominated |
| 1,000 | Clearly more expensive | Usually the cheapest | Close to crossover |
| 10,000 | Not viable | Wear limit approaching | Clearly the cheapest |
The crossover usually sits between 100 and 200 parts for a small plastic part with simple geometry, and moves up towards 500-1,000 when the part needs a polished or textured finish, because the machined part needs hand finishing that the molded part gets free from the tool.
SkillsProto quotes both routes against the same STEP file, so the comparison uses the same geometry rather than two different interpretations of a drawing. That matters more than it sounds: the CNC quote includes the finishing the molded part gets from the tool, and the molding quote includes the draft the CNC quote did not need.
The costs that do not appear on the quotation
Four line items routinely add 10-30% to a project and are invisible on a per-part price:
- Draft and wall-thickness rework. A part designed for machining usually has vertical walls and uniform sections, both of which mold badly. The redesign is engineering time, and it happens after the tool is quoted.
- T1 sample iteration. Aluminium tooling in 7-10 days gets samples in about two weeks. If the first samples need a change, the loop repeats. Two loops is normal; plan for it.
- Scrap during ramp. The first few hundred shots run at a higher reject rate while the process is dialled in. That cost is real and rarely quoted.
- Secondary operations. Threaded inserts, ultrasonic welding, painting, laser marking — none are part of the molding price, and all are part of the delivered part.
A supplier who quotes only the tool and the unit price has quoted about 70% of the project.
How to get a comparable quote in 24 hours
Three inputs decide 90% of the number: a STEP or IGES model, the annual quantity with the expected first-order quantity, and the material with any regulatory constraint (food contact, flame retardancy, UV exposure). Add the surface requirement — cosmetic class A, technical, or hidden — because it changes the tool steel and the polishing time.
SkillsProto returns DFM feedback and a priced quote within 24 hours, with tooling, unit price and lead time on separate lines, and flags the design changes that would reduce the tool cost before any metal is cut. Aluminium tooling runs 7-10 days to first samples, steel 15-25 days, MOQ 1 on the machined prototype that usually precedes the tool.
Send the model at /quote/ and ask for both the machined and the molded route on the same file. The crossover point is the number that decides the project, and it takes one quote to see it.
Frequently Asked Questions
How much does an injection mold cost?
For a small to medium part in a single cavity, aluminium tooling typically sits in the low four figures and a comparable P20 steel tool in the mid to high four figures, in euros. Multi-cavity hardened steel tools run to five figures. The spread within each band is wide because rib thickness, surface finish and undercuts drive machining hours more than part size does, so the only reliable number comes from a quote against the actual model.
Is aluminium tooling good enough for 1,000 parts?
Yes. A 7075 aluminium cavity comfortably runs a few thousand shots of unfilled plastic, so 1,000 parts is well inside its life. It reaches first samples in 7-10 days against 15-25 days for steel, which is usually worth more than the tool life it gives up. Move to steel when the volume passes roughly 10,000 parts, when the material is glass-filled, or when the tool must hold a Class A surface for the whole run.
Why is the unit price lower at higher quantity?
Three reasons compound. Tooling is amortised over more parts, machine setup is spread across a longer run, and the shop can justify a multi-cavity tool or a hot runner that cuts cycle time. The unit price does not fall forever: below a certain point it is material and machine time, and neither scales with volume.
At what quantity is injection molding cheaper than CNC machining?
For small plastic parts with simple geometry the crossover is usually between 100 and 200 parts. It moves up towards 500-1,000 when the part needs a polished or textured surface, because a machined part needs hand finishing that a molded part inherits from the tool. Above 1,000 parts molding is almost always cheaper per part; below 100, machining is.
What drives injection molding cost more than anything else?
Wall thickness. It sets cooling time, which sets cycle time, which sets the machine hour content of every part. A 3.5 mm wall can take three times as long to cool as a 2.5 mm wall, and the cost difference across a production run exceeds most material savings. Wall thickness is also free to change on a drawing, which makes it the highest-leverage decision in the design.
How long does it take to get molded parts?
Aluminium tooling takes 7-10 days to cut and reaches T1 samples at about two weeks; steel tooling takes 15-25 days to cut with samples a week or so after that. Add 3-5 days for DDP delivery to the UK, EU or North America. If the schedule is tighter than that, a CNC machined prototype in 3-7 days is the bridge, and SkillsProto quotes both routes from the same file.
Related capabilities
Related guides
Have parts to quote?
Upload your files — DFM-checked quotation within 24 hours.