Polypropylene (PP)

Polypropylene is cheap, chemically resistant and remarkable in fatigue, which is why it dominates living hinges, containers, lids and fluid handling parts. It is a semicrystalline resin with high shrinkage, so mould design has to account for it early.

ファイルをアップロード — 24時間で見積もり  DFMレビューを依頼

能力

対応内容

Excellent chemical resistance to acids and bases

Excellent chemical resistance to acids and bases

Superb fatigue life, ideal

Superb fatigue life, ideal for living hinges

Low density, so parts are light and cheap

Low density, so parts are light and cheap

Food contact and medical grades available

Food contact and medical grades available

Good impact strength, especially at low temperature

Good impact strength, especially at low temperature

Moulded, machined, welded and thermoformed

Moulded, machined, welded and thermoformed

材料

材料

Homopolymer PP
Copolymer PP
Glass-filled PP
Talc-filled PP
PP sheet and rod
Food contact grades
仕様

主要仕様

項目詳細
Tensile strength33 MPa
Impact strengthNotched Izod 25–60 J/m
Heat deflection100 °C at 0.45 MPa
Density0.905 g/cm³
Shrinkage1.0–2.5 % (high)
ChemicalExcellent, non-polar
仕上げ

表面処理・後加工

Moulded-in texture

Moulded-in texture

Painting with PP primer

Painting with PP primer

Ultrasonic welding

Ultrasonic welding

Laser marking

Laser marking

FAQ

よくあるご質問

Why is PP hard to glue and paint?

Its non-polar surface resists adhesion, so parts need flame, plasma or primer treatment before bonding or painting. We specify the treatment in the process plan.

What is a living hinge?

A thin PP section that flexes thousands of times without breaking, which is why PP dominates flip-top lids and clip designs. Living hinges must be designed in the flow direction of the mould.

Does PP shrink a lot?

Yes, between 1 and 2.5 %, which is much higher than ABS. Moulds and cooling are designed around that shrinkage, and wall thickness consistency matters more than with other resins.